Flogen
2019 - Sustainable Industrial Processing Summit & Exhibition
23-27 October 2019, Coral Beach Resort, Paphos, Cyprus
Abstract still accepted for a limited time
Almost 500 Abstracts Submitted from 60 Countries
Six Nobel Laureates have already confirmed their attendance: Profs. Dan Shechtman, Kurt Wüthrich, Ferid Murad, Rudy Marcus, Yuan Lee and Klaus Klitzing.
NEWS
Abstract Submission
Login
PLENARY LECTURES AND VIP GUESTS
no_photo

Marko Soderžnik

Jožef Stefan Institute

Towards High Coercivities In Heavy Rare Earth Free Nd-fe-b Ribbons
Kobe International Symposium on Science of Innovative and Sustainable Alloys and Magnets (5th Intl. Symp. on Science of Intelligent and Sustainable Advanced Materials (SISAM))

Back to Plenary Lectures »

Abstract:

Reasonable magnetic performance to weight ratio makes polymer-bonded magnets indispensable in automotive applications [i]. The magnetic powders, used for bonded magnets are mainly produced by the gas atomization and melt-spinning [ii]. Several magnetic powders can be used for such purposes, namely ferrites, SmCo, Sm-Fe-N, Nd-Fe-B and/or combinations of all of them. Since the magnetic powder is blended with non-magnetic binder, the remanent magnetization is diluting as the volume percent of the binder is increasing. Therefore, they can be classified as medium-performance isotropic bonded magnets. The coercivity of the magnet, however, is not related to the magnetic powder/non-magnetic binder ratio but to the chemistry and microstructural features. Melt-spun ribbons of Nd-Fe-B material are composed of randomly oriented Nd2Fe14B grains within the size of single magnetic domain [iii]. Therefore, they have a huge potential for higher coercivity compared to sintered Nd-Fe-B magnets in which a typical grain size is measured in microns [iv]. There exist several ways to improve the coercivity of Nd-Fe-B magnets. One way is to decouple the Nd2Fe14B grains by infiltration of low eutectic Nd-based alloys which we propose within this study. Detailed microstructural analyses showed that non-ferromagnetic Nd70Cu30 was successfully infiltrated between the grains, which prevented the physical contact between the grains leading to weaker intergrain exchange coupling. The results of such a process show more than 20 % improvement in coercivity while the remanence is increased as expected due to the lower amount of the ferro-magnetic phase. Significant increase in coercivity compensates lower remanence, and the energy product is also increased. In comparison to the basic powder, the coercivity at 150 °C is significantly improved, which enables these magnets to be used at a higher temperature.

References:

[i] J. J. Croat, 8-Major applications for rapidly solidified NdFeB permanent magnets, Woodhead Publishing Series in Electronic and Optical Materials (2018) 325–361.
[ii] G. Sarriegui, J. M. Martín, M. Ipatov, A. P. Zhukov, J. Gonzalez, Magnetic Properties of NdFeB Alloys Obtained by Gas Atomization Technique, IEEE Trans. Magn. 54 (2018) 2103105.
[iii] J. D. Livingston, Magnetic domains in sintered Fe-Nd-B magnets, J. Appl. Phys. 57 (1985) 4137–4139.
[iv] M. Soderžnik, M. Korent, K. Žagar Soderžnik, M. Katter, K. Üstüner, S. Kobe, Acta Mat. 115 (2016) 178–284.